Product Details

Chemical composition


C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Cu(%) Thick (mm) Yield stress (Mpa) Tensile stress (Mpa)
≦0.12 ≦0.12 ≦0.12 ≦0.12 ≦0.12 ≦0.12 ≦0.12 ≦0.12 ≦0.12 ≦0.12


Applications

Superior Atmospheric Corrosion Resisting Rolled Steels


Country Code:

CNS

Standard

4620

Steel Type

SPA-H

Heat treatment

Heat Treatment of steel grade SPA-C
Heat treated : 1987°C - 1415°C


Relate Steel Type

Steel Type Standard Country Code C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Cu(%)
≦0.04 0.30-1.25 0.25-0.60
SPA-H 4620 CNS ≦0.12 0.25-0.75 0.20-0.50 0.07-0.15 ≦0.04 0.30-1.25 0.25-0.60
SPA-H G3125 JIS ≦0.12 0.25-0.75 0.20-0.50 0.07-0.15 ≦0.04 0.30-1.25 0.25-0.60
Type1 A242 ASTM ≦0.15 ≦1.00 ≦0.15 ≦0.04 0.30-1.25 0.25-0.60


Related Products

SPA-H SPA-C Type1 SPA-C SPA-H


Other Products Catalog


Corrosion-Resisting and Heat-Resisting Superalloy Sheets Plates and Bars
Magnesium Alloy Pipes And Tubes
Magnesium Alloy Shapes
Magnesium Alloy Castings
Magnesium Alloy Die Castings


Other Catalog Products item

Gr.WCB 1033 14NiCr14 MB3 C7541W S 18-1-2-5 100Mn-CrV4 17Mn4 AlBC2/AlBC2C CuZn40