Chemical composition


C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Yield stress (Mpa) Tensile stress (Mpa) Elongation (%)
C(%)(%) 0.9-1.3 Si(%)(%) ≦0.8 0.9-1.3 P(%)(%) ≦0.07 S(%)(%) ≦0.04 0.9-1.3 0.9-1.3 0.9-1.3 0.9-1.3 0.9-1.3


Applications

High Manganese Steel Casting


Country Code:

CNS

Standard

3830

Steel Type

SCMnH11

Heat treatment

Heat Treatment of steel grade SCMnH11
Heat treated : 1412°C - 1766°C


Relate Steel Type

Steel Type Standard Country Code C(%) V(%) Si(%) Mn(%) P(%) S(%) Cr(%)
SCMnH11 3830 CNS 0.9-1.3 ≦0.8 11.0-14.0 ≦0.07 ≦0.04 1.5-2.5
SCMnH21 3830 CNS 1.00-1.35 0.4-0.7 ≦0.8 11.0-14.0 ≦0.07 ≦0.04 2.0-3.0
ZGMn13-4(GB) GB 0.9-1.3 0.3-1.0 11.0-14.0 ≦0.07 ≦0.04 1.5-2.5
SCMnH11 G5131 JIS 0.9-1.3 ≦0.8 11.0-14.0 ≦0.07 ≦0.04 1.5-2.5
SCMnH21 G5131 JIS 1.00-1.35 0.4-0.7 ≦0.8 11.0-14.0 ≦0.07 ≦0.04 2.0-3.0
C A128 ASTM 1.05-1.35 ≦1.0 11.5-14.0 ≦0.07 1.5-2.5
GX120-Mn12 17145 DIN 1.1-1.3 0.3-0.5 12.0-13.0 ≦0.1 ≦0.04 ≦1.5


Related Products

SCMnH11 ZGMn13-1(GB) SCMnH1 B1 B4 SCMnH21 SCMnH21 SCMnH3 SCMnH2 SCMnH3
X110Mn14 SCMnH11 ZGMn13-3(GB) ZGMn13-4(GB) SCMnH1 ZGMn13-2(GB) SCMnH2 B2 B2


Other Products Catalog


Alloy Steel Bars for Special Application Bolting Materials
Zinc Alloy Castings
Titanium and Titanium Alloy Sheets,Plates and Strips
Titanium and Titanium Alloy Seamless Pipes
Titanium and Titanium Alloy Tube for Heat Exchangers


Other Catalog Products item

NiCr20Ti-A1 A2017BD AlCuSiMn KmTBCr9-Ni55i2 AZ61A SUM42 S 18-0-1 CuNi10Fe1Mn 6 1050