Chemical composition


C(%) Si(%) Mn(%) P(%) S(%) Yield stress (Mpa) Tensile stress (Mpa) Elongation (%)
C(%)(%) 0.25-0.35 Si(%)(%) 0.3-0.6 0.25-0.35 P(%)(%) <=0.04 S(%)(%) <=0.04 0.25-0.35 0.25-0.35 0.25-0.35 0.25-0.35 0.25-0.35


Applications

High Tensile Strength Carbon Steel Castings and Low Alloy Steel Castings for Structur


Country Code:

JIS

Standard

G5111

Steel Type

SCMn2A

Heat treatment

Heat Treatment of steel grade JIS SCMn 3
Heat treated : 1455°C - 1432°C


Relate Steel Type

Steel Type Standard Country Code C(%) Si(%) Mn(%) P(%) S(%) Yield stress (Mpa) Tensile stress (Mpa)
SCMn2A 7145 CNS 0.25-0.35 0.3-0.6 1.0-1.6 <=0.04 <=0.04 >=345 >=590
SCMn2A G5111 JIS 0.25-0.35 0.3-0.6 1.0-1.6 <=0.04 <=0.04 >=345 >=590
GS-30Mn5 1681 DIN 0.27-0.34 0.3-0.50 1.2-1.5 <=0.035 <=0.035


Related Products

SCCrM3A GS-60 SCMnM3B SCMnCr-M3A SCNCr-M2B SCC5B SCMn2A GS-36Mn5 SCMn1B GS-34CMo4
105-85 SCCrM3B SCMn5B SCC3B 90-60 SCSiMn2B SCMnCr-M2A SCMn1B SCMnM3B SCMnM3B


Other Products Catalog


Titanium and Titanium Alloy Tube for Heat Exchangers
Titanium and Titanium Alloy Rods and Bars
Bronze Castings
Phosphor Bronze Castings
Leaded Bronze Castings


Other Catalog Products item

H II 1320 A5052S SCPL31 G-X40Ni-CrSi36-18 Class F 6061 Gr.F ZL107 MP4