Product Details

Chemical composition


C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) Ni(%) Yield stress (Mpa) Tensile stress (Mpa)
C(%)(%) 0.2-0.4 Si(%)(%) ≦0.2 0.2-0.4 P(%)(%) ≦0.04 S(%)(%) ≦0.04 0.2-0.4 0.2-0.4 0.2-0.4 0.2-0.4 0.2-0.4


Applications

Heat Resisting Steel Castings


Country Code:

CNS

Standard

4002

Steel Type

SCH12

Heat treatment

Heat Treatment of steel grade SCH12
Heat treated : 1769°C - 1148°C


Relate Steel Type

Steel Type Standard Country Code C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%)
SCH12 4002 CNS 0.2-0.4 ≦0.2 ≦0.2 ≦0.04 ≦0.04 18.0-23.0 ≦0.5
SCH12 G5122 JIS 0.2-0.4 ≦2.0 ≦2.0 ≦0.04 ≦0.04 18.0-23.0 ≦0.5
HF A297 ASTM 0.2-0.4 ≦2.0 ≦2.0 ≦0.04 ≦0.04 18.0-23.0 ≦0.5
G-X40Cr-NiSi22-9 17465 DIN 0.3-0.5 1.0-2.0 0.5-1.5 ≦0.045 ≦0.03 21.0-23.0


Related Products

SCH18 ZG30Ni35-Cr15 SCH15 SCH2 G-X40Cr-NiSi25-20 SCH19 HE HK40 SCH13A HF
HN SCH2 SCH3 G-X40Ni-CrSi36-18 HX SCH13A ZG40Cr25-Ni20 SCH23 SCH11 SCH11


Other Products Catalog


Titanium and Titanium Alloy Rods and Bars
Bronze Castings
Phosphor Bronze Castings
Leaded Bronze Castings
Corrosion-Resisting Stainless Steels


Other Catalog Products item

St14-05 10SPb20 28Mn6 Gr.3 2018FD SUM22L L1 SCPL31 EZ33A Class 1