Product Details

Chemical composition


C(%) Si(%) Mn(%) P(%) S(%) Yield stress (Mpa) Tensile stress (Mpa) Elongation (%)
C(%)(%) 0.3-0.4 Si(%)(%) 0.3-0.6 0.3-0.4 P(%)(%) <=0.04 S(%)(%) <=0.04 0.3-0.4 0.3-0.4 0.3-0.4 0.3-0.4 0.3-0.4


Applications

High Tensile Strength Carbon Steel Castings and Low Alloy Steel Castings for Structur


Country Code:

CNS

Standard

7145

Steel Type

SCC3B

Heat treatment

Heat Treatment of steel grade SCC3
Heat treated : 1464°C - 1823°C


Relate Steel Type

Steel Type Standard Country Code C(%) Si(%) Mn(%) P(%) S(%) Yield stress (Mpa) Tensile stress (Mpa)
SCC3B 7145 CNS 0.3-0.4 0.3-0.6 0.5-0.8 <=0.04 <=0.04 >=131 >=370
SCC3B G5111 JIS 0.3-0.4 0.3-0.6 0.5-0.8 <=0.04 <=0.04 >=131 >=370
GS-60 1681 DIN 0.4-0.4 0.3-0.6 0.2-0.5 <=0.04 <=0.04 >=300 >=600


Related Products

SCC3B SCC3A GS-46Mn4 GS-70 SCSiMn2B SCC5B GS-30Mn5 SCMn3A SCMnCr-M2A SCMn5A
28Mn6 SCNCr-M2A SCC3A SCMnCr-M2B SCCrM3A GS-60 SCMnM3B SCMnCr-M3A SCNCr-M2B SCNCr-M2B


Other Products Catalog


Heat Resisting Steel Castings
Gray lron Castings
Spheroidal Graphite lron Castings
Austenitic Cast lron of Flake Graphite
Austenitic Cast lron of Spheroidal Graphite


Other Catalog Products item

T2 C26000 35CrMnSiA CuZn40 SCH24 A2017TE SMA490AW SQV3A Gr.23 C7701W