Chemical composition


C(%) Si(%) Al(%) Mn(%) P(%) S(%) Ti(%) Cr(%) Ni(%) Cu(%)
≦0.1 ≦0.1 ≦0.1 ≦0.1 ≦0.1 ≦0.1 ≦0.1 ≦0.1 ≦0.1 ≦0.1


Applications

Corrosion-Resisting and Heat-Resisting Superalloy Sheets Plates and Bars


Country Code:

CNS

Standard

NCF800

Steel Type



Heat treatment

Heat Treatment of steel grade VV-54
Heat treated : 1391°C - 1967°C


Relate Steel Type

Steel Type Country Code C(%) Si(%) Al(%) Mn(%) P(%) N(%) S(%) Ti(%)
≦0.15 0.15-0.60
NCF800 CNS ≦0.1 ≦1.0 0.15-0.60 ≦1.5 ≦0.03 ≦0.15 0.15-0.60
GH20 GB ≦0.1 ≦1.0 ≦1.5 ≦0.045 ≦0.15 0.15-0.60
NCF800B JIS ≦0.1 ≦1.0 0.15-0.60 ≦1.5 ≦0.03 ≦0.15 0.15-0.60
X10NiCr-A1Ti32-20 DIN ≦0.12 ≦1.0 0.15-0.60 ≦2.0 ≦0.03 ≦0.15 0.15-0.60


Related Products

NCF751 NCF751 NCF800H NCF825 NiCr-15Fe NCF601 NiCr20Ti-A1 NCF825 NCF600 X10NiCr-A1Ti32-20
NCF80A NCF750 NCF600B NCF601 GH145 NCF800B GH80A GH80A


Other Products Catalog


Copper-Nickel-Zinc (Nickel Silver) Alloy Wires
Carbon Steels and Manganese Steels for Machine Structural use
Carbon Steel and Molybdenum Alloy Steel Plates for Boilers and OtherPressureVessels
Carbon Steel Forgings for General use
Carbon Steel Forgings for Pressure Vessels


Other Catalog Products item

20Mn5 Ti 3 Al 99.5 SQV1B C17200 30CrNi3 C53400 StW22 SNB24-3 SCPH11