C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Fe(%) | Ni(%) | Cu(%) | Yield stress (Mpa) | ≦0.15 | ≦0.15 | ≦0.15 | ≦0.15 | ≦0.15 | ≦0.15 | ≦0.15 | ≦0.15 | ≦0.15 | ≦0.15 |
---|
Corrosion-Resisting and Heat-Resisting Superalloy Sheets Plates and Bars
Steel Type | Country Code | C(%) | Si(%) | Al(%) | Mn(%) | P(%) | S(%) | Cr(%) | Fe(%) | ≦0.015 | 14.0-17.0 | 6.0-10.0 | NCF600 | CNS | ≦0.15 | ≦0.5 | ≦1.0 | ≦0.03 | ≦0.015 | 14.0-17.0 | 6.0-10.0 | NCF600B | JIS | ≦0.15 | ≦0.5 | ≦1.0 | ≦0.03 | ≦0.015 | 14.0-17.0 | 6.0-10.0 | NiCr-15Fe | DIN | 0.05-0.1 | ≦0.5 | ≦0.3 | ≦1.0 | ≦0.02 | ≦0.015 | 14.0-17.0 | 6.0-10.0 |
---|
NiCr15Fe-7TiA1 | NCF600B | NCF601 | GH145 | NCF800B | GH80A | NCF800 | NCF800H | GH20 | NCF750B | NCF751 | NCF751 | NCF800H | NCF825 | NiCr-15Fe | NCF601 | NiCr20Ti-A1 | NCF825 | NCF825 |
C93700 | LF11 | SEV245 | 1330 | MgAl3Zn | SUS416 | C2700T | CuSn10 | GGL-Ni-Cr20-2 | 20Cr |