C(%) |
Si(%) |
Mn(%) |
P(%) |
N(%) |
S(%) |
| | | | | | | ≦0.035 | | ≦0.035 |
| SM400B | 2947 | CNS | ≦0.20 | ≦0.35 | 0.60-1.40 | ≦0.035 | | ≦0.035 |
| Q235B | T700 | GB | 0.12-0.20 | ≦0.30 | 0.30-0.70 | ≦0.035 | | ≦0.035 |
| SM400B | G3106 | JIS | ≦0.20 | ≦0.35 | 0.60-1.40 | ≦0.035 | | ≦0.035 |
| Gr.D | A284 | ASTM | ≦0.27 | 0.15-0.40 | ≦0.90 | ≦0.035 | | ≦0.035 |
| RSt42-2 | 17100 | DIN | ≦0.25 | | 0.20-0.50 | ≦0.035 | | ≦0.035 |
| St42-3U | 17100 | DIN | ≦0.23 | 0.03-0.30 | 0.20-0.50 | ≦0.035 | | ≦0.035 |
| St44-2 | 17100 | DIN | ≦0.21 | | | ≦0.035 | | ≦0.035 |
| St44-3 | 17100 | DIN | ≦0.20 | | | ≦0.035 | | ≦0.035 |