C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Tensile stress (Mpa) | Elongation (%) | C(%)(%) 0.3-0.5 | Si(%)(%) 1.0-2.0 | 0.3-0.5 | P(%)(%) ≦0.045 | S(%)(%) ≦0.03 | 0.3-0.5 | 0.3-0.5 | 0.3-0.5 | 0.3-0.5 | 0.3-0.5 |
---|
Heat Resisting Steel Castings
Steel Type | Standard | Country Code | C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | SCH13 | 4002 | CNS | 0.2-0.5 | ≦2.0 | ≦2.0 | ≦0.04 | ≦0.04 | 24.0-28.0 | ≦0.5 | SCH13A | 4002 | CNS | 0.25-0.5 | ≦1.75 | ≦2.5 | ≦0.04 | ≦0.04 | 23.0-26.0 | ≦0.5 | ZG35Cr26-Ni12 | 8492 | GB | 0.2-0.5 | ≦2.0 | ≦2.0 | ≦0.04 | ≦0.03 | 24.0-28.0 | SCH13 | G5122 | JIS | 0.2-0.5 | ≦2.0 | ≦2.0 | ≦0.04 | ≦0.04 | 24.0-28.0 | ≦0.5 | SCH13A | G5122 | JIS | 0.25-0.5 | ≦1.75 | ≦2.5 | ≦0.04 | ≦0.04 | 23.0-26.0 | ≦0.5 | HH | A297 | ASTM | 0.2-0.5 | ≦2.0 | ≦2.0 | ≦0.04 | ≦0.04 | 24.0-28.0 | G-X40Cr-NiSi22-9 | 17465 | DIN | 0.3-0.5 | 1.0-2.0 | 0.5-1.5 | ≦0.045 | ≦0.03 | 21.0-23.0 | SCH12 | 4002 | CNS | 0.2-0.4 | ≦0.2 | ≦0.2 | ≦0.04 | ≦0.04 | 18.0-23.0 | ≦0.5 | SCH12 | G5122 | JIS | 0.2-0.4 | ≦2.0 | ≦2.0 | ≦0.04 | ≦0.04 | 18.0-23.0 | ≦0.5 | HF | A297 | ASTM | 0.2-0.4 | ≦2.0 | ≦2.0 | ≦0.04 | ≦0.04 | 18.0-23.0 | ≦0.5 |
---|
SCH2 | G-X40Cr-NiSi25-20 | SCH19 | HE | HK40 | SCH13A | HF | HN | SCH2 | SCH3 | G-X40Ni-CrSi36-18 | HX | SCH13A | ZG40Cr25-Ni20 | SCH23 | SCH11 | HU | SCH21 | G-X40Cr-NiSi27-4 | G-X40Cr-NiSi27-4 |
SMA570W | GGG-Ni-Mn13-7 | TA1 | G-CuZn25Al5 | SNB24-1 | C51000 | SCW49 | 1065 | PBC2B | 80WCrV8 |