Product Details

Chemical composition


C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) Ni(%) Yield stress (Mpa) Tensile stress (Mpa)
C(%)(%) 0.04-0.20 Si(%)(%) ≦1.75 0.04-0.20 P(%)(%) ≦0.04 S(%)(%) ≦0.04 0.04-0.20 0.04-0.20 0.04-0.20 0.04-0.20 0.04-0.20


Applications

Stainless Steel Castings


Country Code:

ASTM

Standard

A743

Steel Type

CK-20

Heat treatment

Heat Treatment of steel grade CK-20
Heat treated : 1154°C - 1347°C


Relate Steel Type

Steel Type Standard Country Code C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%)
SCS18 4000 CNS ≦0.2 ≦2.0 ≦2.0 ≦0.04 ≦0.04 23.0-27.0
SCS18 G5121 JIS ≦0.2 ≦2.0 ≦2.0 ≦0.04 ≦0.04 23.0-27.0
CK-20 A743 ASTM 0.04-0.20 ≦1.75 ≦1.5 ≦0.04 ≦0.04 23.0-27.0 ≦0.5


Related Products

SCS3 SCS3 SCC13 CF-3M SCS14A ZG0Cr-18Ni9 SCS21 SCS17 CA-40 CF-20
SCS4 SCS10 SCS2 CK-20 ZG1Cr-18Ni9 SCS18 SCS6 G-X6CrNi-Mo18-10 SCS13A SCS13A


Other Products Catalog


Bearing Steels
Superior Atmospheric Corrosion Resisting Rolled Steels
Corrosion-Resisting and Heat-Resisting Superalloy Sheets Plates and Bars
Magnesium Alloy Pipes And Tubes
Magnesium Alloy Shapes


Other Catalog Products item

C44300 - 35Cr 1108 ZCuZn16Si4 SM520B AZ91A SCH15 12CrNi4 BZn 15-20