Product Details

Chemical composition


Mn(%) Pb(%) Fe(%) Ni(%) Zn(%) Cu(%)
≦0.5 ≦0.5 ≦0.5 ≦0.5 ≦0.5 ≦0.5 ≦0.5 ≦0.5 ≦0.5 ≦0.5


Applications

Copper-Nickel-Zinc (Nickel Silver) Alloy Rods


Country Code:

CNS

Standard

10441

Steel Type

C7521B

Heat treatment

Heat Treatment of steel grade C75S
Heat treated : 1718°C - 1351°C


Relate Steel Type

Steel Type Standard Country Code Mn(%) Pb(%) Fe(%) Ni(%) Zn(%) Cu(%) More
≧12.0 61.0-67.0 More
C7521B 10441 CNS ≦0.5 ≦0.1 ≦0.25 16.5-19.5 ≧12.0 61.0-67.0 More
C7521B H3270 JIS ≦0.5 ≦0.1 ≦0.25 13.5-15.5 ≧12.0 61.0-67.0 More
C75200 B151 ASTM ≦0.5 ≦0.05 ≦0.25 16.5-19.5 ≧12.0 61.0-67.0 More
CuNi18Zn20 17663 DIN ≦0.5 ≦0.03 ≦0.3 17.0-19.0 ≧12.0 61.0-67.0 More


Related Products

C7941B C7541P/C7541R C75200 C7541W C7451P/C7451R C7941B C7701B C7541W C75200
C7541P/C7541R C7521P/C7521R C7541B C7541B C75200 C7451W C7521B C7521W C7701B C7701B


Other Products Catalog


Carbon Steel and Molybdenum Alloy Steel Plates for Boilers and OtherPressureVessels
Carbon Steel Forgings for General use
Carbon Steel Forgings for Pressure Vessels
Quenched and Tempered Alloy Steel Forgings for Pressure Vessels
Alloy Steel Forgings for Pressure Vessels for High Temperature Service


Other Catalog Products item

C7941B C5101W KTH300-06 FCMP440 2014 G-MgSE3Zn2Zr1 SFVC2A StW22 C5191P/C5191R AZ91A