Chemical composition
Applications
Structural Steels with Specified Hardenability Bands
Country Code:
GB
Standard
6479
Steel Type
15CrMo
Heat treatment
Heat Treatment of steel grade 15CrMo4
Heat treated : 1926°C - 1664°C
Relate Steel Type
Inquiry |
Steel Type |
Standard |
Country Code |
C(%) |
Si(%) |
Mn(%) |
P(%) |
S(%) |
Cr(%) |
| | | | | | | ≦0.03 | ≦0.03 | 0.85-1.25 |
| SCM415H | 11999 | CNS | 0.12-0.18 | 0.15-0.35 | 0.55-0.90 | ≦0.03 | ≦0.03 | 0.85-1.25 |
| 15CrMo | 6479 | GB | 0.12-0.18 | 0.17-0.37 | 0.4-0.7 | ≦0.03 | ≦0.03 | 0.85-1.25 |
| SCM415H | G4052 | JIS | 0.12-0.18 | 0.15-0.35 | 0.55-0.90 | ≦0.03 | ≦0.03 | 0.85-1.25 |
| 4118H | A304 | ASTM | 0.17-0.23 | 0.15-0.35 | 0.6-1.0 | ≦0.03 | ≦0.03 | 0.85-1.25 |
| 4118H | - | AISI | 0.18-0.23 | 0.15-0.30 | 0.7-0.9 | ≦0.03 | ≦0.03 | 0.85-1.25 |
| 15CrMo5 | 17200 | DIN | 0.13-0.17 | 0.15-0.35 | 0.5-1.1 | ≦0.03 | ≦0.03 | 0.85-1.25 |