Chemical composition
C(%)
Si(%)
Mn(%)
P(%)
S(%)
Cr(%)
Ni(%)
¨Q0.03 ¨Q1.0 ¨Q2.0 ¨Q0.045 ¨Q0.03 18.0-20.0 10.0-12.0
Applications
- X2CrNi 19-11 Austenitic Cr-Ni steel, non-hardenable, particularly suitable for welded structures. Excellent intercrystalline corrosion resistance, usable up to about 400 degree Celsius. Used for welded structures and where intercrystalline strength is required.
Application: Automotive, Chemical / Petrochemical, Energy, Fixings / Bolts, Food / Pharmaceuticals, Hydraulics / Couplings
Country Code
- DIN
Standard
- 2CrNi-19-11
Steel Type
X2CrNi-19-11
Heat treatment
Hot forming temp : 1200 -- 900degree Celsius
Heat treatment temperature and cooling methods|quenching:1000-- 1100 degree Celsius, air/water cooled
Relate Steel Type
Steel Type | Country Code | C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) |
---|---|---|---|---|---|---|---|---|
304L | CNS | ¨Q0.03 | ¨Q1.0 | ¨Q2.0 | ¨Q0.045 | ¨Q0.03 | 18.0-20.0 | 9.0-13.0 |
00Cr19-Ni10 | GB | ¨Q0.03 | ¨Q1.0 | ¨Q2.0 | ¨Q0.035 | ¨Q0.03 | 18.0-20.0 | 9.0-13.0 |
SUS304L | JIS | ¨Q0.03 | ¨Q1.0 | ¨Q2.0 | ¨Q0.045 | ¨Q0.03 | 18.0-20.0 | 9.0-13.0 |
304L | AISI | ¨Q0.03 | ¨Q1.0 | ¨Q2.0 | ¨Q0.045 | ¨Q0.03 | 18.0-20.0 | 8.0-10.5 |
X2CrNi-19-11 | DIN | ¨Q0.03 | ¨Q1.0 | ¨Q2.0 | ¨Q0.045 | ¨Q0.03 | 18.0-20.0 | 10.0-12.0 |