X12Cr-Ni18-8

Chemical composition

C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%)
¨Q0.12 ¨Q1.0 ¨Q2.0 ¨Q0.045 ¨Q0.03 17.0-19.0 8.0-10.0

Applications

  • X12Cr-Ni18-8 is a kind of stainless steel, executive standard: DIN EN 10088-3
    Stainless Steel Wire for Spring use
    Corrosion-Resisting Stainless Steels

Country Code

  • DIN

Standard

  • 12Cr-Ni18-8


Steel Type
X12Cr-Ni18-8

Heat treatment
Solution annealing : 1000 - 1100 degree Celsius (water)

Relate Steel Type

Steel Type Country Code C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%)
302 CNS ¨Q0.15 ¨Q1.0 ¨Q2.0 ¨Q0.045 ¨Q0.03 17.0-19.0 8.0-10.0
1Cr18Ni9 GB ¨Q0.15 ¨Q1.0 ¨Q2.0 ¨Q0.035 ¨Q0.03 17.0-19.0 8.0-10.0
SUS302 JIS ¨Q0.15 ¨Q1.0 ¨Q2.0 ¨Q0.045 ¨Q0.03 17.0-19.0 8.0-10.0
302 ASTM ¨Q0.15 ¨Q1.0 ¨Q2.0 ¨Q0.045 ¨Q0.03 17.0-19.0 8.0-10.0
X12Cr-Ni18-8 DIN ¨Q0.12 ¨Q1.0 ¨Q2.0 ¨Q0.045 ¨Q0.03 17.0-19.0 8.0-10.0
302 AISI ¨Q0.15 ¨Q1.0 ¨Q2.0 ¨Q0.045 ¨Q0.03 17.0-19.0 8.0-10.0