Chemical composition
C(%)
Si(%)
Mn(%)
P(%)
S(%)
Cr(%)
Ni(%)
¨Q0.15 ¨Q1.0 ¨Q2.0 ¨Q0.045 ¨Q0.03 16.0-18.0 6.0-8.0
Applications
- SUS301 stainless steel can obtain high strength after cold working. SUS301 stainless steel is used in railway vehicles, belt conveyors, bolts and nuts, springs, etc.
Country Code
- JIS
Standard
- US301
Steel Type
SUS301
Heat treatment
Heat treatment temperature : 1010--1150 degree Celsius
Medium: rapid cooling
σb/>= MPa: 520
σ0.2/>= MPa: 205
δ >=(%): 40
Ñ„ >= (ï¼…): 60
Hardness | HB >=: 207
Relate Steel Type
Steel Type | Country Code | C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) |
---|---|---|---|---|---|---|---|---|
301 | CNS | ¨Q0.15 | ¨Q1.0 | ¨Q2.0 | ¨Q0.045 | ¨Q0.03 | 16.0-18.0 | |
1Cr17Ni7 | GB | ¨Q0.15 | ¨Q1.0 | ¨Q2.0 | ¨Q0.035 | ¨Q0.03 | 16.0-18.0 | |
SUS301 | JIS | ¨Q0.15 | ¨Q1.0 | ¨Q2.0 | ¨Q0.045 | ¨Q0.03 | 16.0-18.0 | |
301 | AISI | ¨Q0.15 | ¨Q1.0 | ¨Q2.0 | ¨Q0.045 | ¨Q0.03 | 16.0-18.0 | |
X12Cr-Ni17-7 | DIN | ¨Q0.12 | ¨Q1.5 | ¨Q2.0 | 16.0-18.0 | ¨Q0.8 |