Chemical composition

C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) Ni(%) Cu(%)
¨Q0.08 ¨Q1.0 ¨Q2.0 ¨Q0.045 ¨Q0.03 17.0-19.0 1.20-2.75 12.0-16.0 1.00-2.50

Applications

  • Corrosion-Resisting Stainless Steels

Country Code

  • CNS

Standard

  • 16J1L


Steel Type
316J1L

Heat treatment


Relate Steel Type

Steel Type Country Code C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%)
316J1L CNS ¨Q0.08 ¨Q1.0 ¨Q2.0 ¨Q0.045 ¨Q0.03 17.0-19.0 1.20-2.75
00Cr18Ni-14Mo2Cu2 GB ¨Q0.03 ¨Q1.0 ¨Q2.0 ¨Q0.035 ¨Q0.03 17.0-19.0 1.20-2.75
SUS316J1L JIS ¨Q0.08 ¨Q1.0 ¨Q2.0 ¨Q0.045 ¨Q0.03 17.0-19.0 1.20-2.75